Enhanced TDS
Identification & Functionality
- Manufactured By
- CASE Ingredients Functions
- Industrial Additives Functions
- Technologies
- Product Families
Features & Benefits
Applications & Uses
- Markets
- Applications
- Application Area
- Compatible Polymers & Resins
- Compatible Substrates & Surfaces
- Coating End Applications
- Industrial Additives End Use
- Ink & Toner End Applications
- Use Level
- 5 - 10% (Inorganic Pigments), 10 - 35% (Organic Pigments), 1 - 3% (Titanium Dioxide), 15 - 75% (Carbon Black)
- Application Information
Special Features and Benefits
DISPERBYK-2155 TF deflocculates pigments and stabilizes them by means of steric hindrance. It prevents a possible coflocculation, which leads to flood- and float-free color in pigment blends. The deflocculating property of the additive results in increased gloss, color strength, transparency or hiding power, and a reduced millbase viscosity.
Recommended Use
Due to its high solids content, DISPERBYK-2155 TF is particularly suitable for high-solid coating systems and floor coatings. The additive is exceptionally compatible with all standard coating binders such as alkyd resins, cellulose nitrate, polyols, chlorinated rubber, epoxides, and polyurethanes. DISPERBYK-2155 TF greatly reduces the viscosity of the millbase which enables a higher pigment content in pigment concentrates.Recommended Levels
Amount of additive (as supplied) based upon pigment:
Inorganic pigments: 5-10%
Titanium dioxide: 1-3%
Organic pigments: 10-35%
Carbon black: 15-75%
The above recommended levels can be used for orientation. Optimal levels are determined through a series of laboratory tests.
Incorporation and Processing Instructions
Wetting and dispersing additives should generally be added to the millbase. Only in this way can they be fully effective. In binder-free dispersion, the solvent components of the millbase should be pre-mixed with the additive while stirring, prior to the addition of the pigment. If the grinds contain binder, the binder, solvent, and additive should be homogenized prior to adding the pigment.
Special Note
Deflocculated pigments have a greater tendency to settle. This applies particularly to inorganic pigments, which have a high density. The use of liquid rheology additives such as RHEOBYK-410 or RHEOBYK-430 in the grinding phase counters this phenomenon.
Properties
- Physical Form
- Typical Properties
Value Units Test Method / Conditions Density (at 20°C) 1.06 g/ml - Refractive Index 1.478 - - Amine Value 48 mg KOH/g - Active Substance 100 % - - SDS Physical and Chemical Properties
Value Units Test Method / Conditions Auto Ignition Tempertaure min. 200 °C DIN 51794 Boiling Point min. 200 °C Derived Flash Point 148 °C Pensky-Martens Melting Point 15 °C Derived Density (at 20°C, 1013 hPa) 1.06 g/cm³ Oscillating U-tube Vapour Pressure (at 20°C) max. 1 hPa Derived Appearance Liquid - - Color Light yellow - - Immiscible In Water - - Odor Characteristic - - pH (Concentration: 1%) 8 - Universal pH-Value Indicator - Composition
Polyglycol polyester modified polyalkylene imine
Regulatory & Compliance
- Chemical Inventories
- OEM Specifications